Distillation of precious Pb and precious Bi

Source of raw materials:

This process is applied for precious lead and bismuth alloy with Ag content <15% and Cu content<2%. The main sources for the raw materials are:

  1. Precious lead alloy of lead anode slime smelting from traditional lead smelting plant;
  2. Precious lead alloy of electrolytic anode slime with high bismuth and lead;
  3. Crude bismuth alloy;
  4. Other crude lead and bismuth alloy with Ag content;


This process is applied for precious lead-base alloy and bismuth-base alloy with high Ag and Cu content and alloy melting point greater than 600 . The main sources for the raw materials are:

  1. Precious lead smelting slags and blowing Ag-Cu-Bi alloy from traditional lead smelting plant; Precious bismuth smelting slags ;
  2. Precious lead from copper anode slime ;
  3. Hydrometallurgical slag smelting alloy during the nickel smelting.
  4. Other lead-base alloy and bismuth-base alloy with high Ag and Cu content

Technological characteristics and finished product indexes:

Brief introduction to continuous vacuum treatment process for precious lead and bismuth

Product 1(vacuum crude silver alloy)

Pb<1%, Bi<1%

Product 2 (vacuum crude lead and bismuth alloy)

Ag<5g/t (or 40g/t), Cu<3g/t

Equipment capacity

8-12tons/24 hrs

Electric power consumption

550—650kwh per ton of material

Labour consumption

1-2 people per shift


Product 1(vacuum crude copper alloy

Pb<1%, Bi<1% and Ag<0.3%

Product 2(vacuum precious lead and bismuth alloy)

Cu<0.5%(To continuous vacuum treatment process)

Equipment capacity

0.5-1ton/furnace

Electric power consumption

1000-1500kwh per ton of material

Labour consumption

flexible


Technical advantages of precious lead vacuum treatment

  1. Can remove lead, bismuth and antimony and reduce the silver separating furnace blowing and slag production;
  2. Has big equipment production capacity, can shorten the production period of silver separation process and increase the output rate of silver;
  3. Produce lead, bismuth and antimony in the form of alloy, depending on the content of components, directly high bismuth-lead electrolysis or antimony removal process can be applied.
  4. Generally high direct recovery rate of element vacuum treatment, less mechanical adhesion loss, high metal comprehensive recovery rate;


Technical advantages of precious bismuth vacuum treatment

  1. Completely replace the process of zinc-adding to remove silver during the bismuth refining process, eliminate zinc consumption, and no silver and zinc slags generated, reduce production costs;
  2. Have big equipment production capacity, can greatly reduce the refining time;
  3. Generally high direct recovery rate of element vacuum treatment, less mechanical adhesion loss, and high metal comprehensive recovery rate;
  4. High degree of automation, more stable product quality, low labor intensity and small labor consumption.


Any questions for technology or equipment,please contact us

CHINA HEADQUARTERS

Add:41st Floor, Xiangshang·Century Xincheng, No. 17 Kaiyuan Road, Xingsha Economic Development Zone, Changsha, Hunan, China. 

Tel:0086 731 85781166

Fax:0086 731 85781199

Skype:pbjoyz

Email:info@unionsum.com

RUSSIA OFFICE

Add:Room 1502,15, Pervomayskayastr., Ekaterinburg620075,Russia

Адрес:Россия, 620075 Екатеринбург, ул. Первомайская 15, офис 1502

Mp:007 982 646 60 50

Email:marketing@unionsum.com

BULGARIA OFFICE

Add:bl 49/D, Yavorov complex, Sofia 1111, Bulgaria

Tel:00359 28717072

Fax:00359 28717072

Mp:00359 899853098

Email:bulgaria@unionsum.com

CONTACT US